Abstract

An aqueous solution of phenolic resin was impregnated through drilled holes in wood, and we manufactured compressed wood with the deformation fixed by the phenolic resin. The methods of impregnation used in this study were an in-liquid platen-pressing method and a vacuum treatment. The effect of the drilled holes on solution retention was examined. Moreover, the control of solution retention was examined under the application of compression drying. The impregnation of resin into the specimens without drilled holes was insufficient, and the deformation could not be fixed. On the other hand, sufficient impregnation was possible in the specimen with drilled holes, and the deformation fixation was observed. At the stage of compression when the solution was squeezed out of the specimen, the solution retention of each specimen was accurately controlled in the specimens with drilled holes. At the stage of compressive deformation and deformation fixation using a hot press, the specimens without drilled holes could not be processed normally because swelling occurred. However, swelling did not occur in the specimens with drilled holes.

References

  1. Norimoto M (1993) Large compressive deformation in wood (in Japanese). Mokuzai Gakkaishi 39:867–874

    Google Scholar 

  2. Inoue M, Kadokawa N, Nishio J, Norimoto M (1993) Permanent fixation of compressive deformation by hygro-thermal treatment using moisture in wood (in Japanese). Wood Res 29:54–61

    Google Scholar 

  3. Inoue M, Norimoto M, Otsuka Y, Yamada T (1991) Surface compression of coniferous wood lumber II. Permanent set of compression wood by low molecular weight phenolic resin and some physical properties of the products (in Japanese). Mokuzai Gakkaishi 37:227–233

    CAS  Google Scholar 

  4. Inoue M, Norimoto M, Otsuka Y, Yamada T (1991) Surface compression of coniferous wood lumber III. Permanent set of the surface compressed layer by a water solution of low molecular weight phenolic resin (in Japanese). Mokuzai Gakkaishi 37:234–240

    CAS  Google Scholar 

  5. Inoue M, Ogata S, Kawai S, Rowell RM, Norimoto M (1993) Fixation of compressed wood using melamine—formaldehyde resin. Wood Fiber Sci 25:404–410

    CAS  Google Scholar 

  6. Ryu JY, Takahashi M, Imamura Y, Sato T (1991) Biological resistance of phenol-resin treated wood. Mokuzai Gakkaishi 37:852–858

    CAS  Google Scholar 

  7. Higuchi M (2006) Impregnation of wood with phenolic resin. Suppression of physical deterioration protects wood from termite-attack and decay (in Japanese). Wood Ind 61:238–243

    CAS  Google Scholar 

  8. Adachi K, Inoue M, Kawai S, Kanayama K (2003) Liquid impregnation in dry wood using a roller-pressing method I. Effects of transverse compressive deformation on liquid impregnation (in Japanese). Mokuzai Gakkaishi 49:416–422

    CAS  Google Scholar 

  9. Adachi K, Inoue M, Kawai S (2004) Liquid impregnation into dry wood using a roller-pressing method II. Effects of specimen sizes and processing variables on amount of water impregnation (in Japanese). Mokuzai Gakkaishi 50:243–247

    CAS  Google Scholar 

  10. Adachi K, Inoue M, Kawai S (2005) Liquid impregnation in green wood using a roller-pressing method (in Japanese). Mokuzai Gakkaishi 51:159–165

    Article  CAS  Google Scholar 

  11. Iida I, Takayama C, Miyagawa O, Imamura Y (1992) Liquid penetration of precompressed wood I. Effects of compressive deformation and recovery upon liquid uptake (in Japanese). Mokuzai Gakkaishi 38:233–240

    Google Scholar 

  12. Iida I, Imamura Y, Kashiwa N, Nakamura Y (1992) Liquid penetration of precompressed wood II. Effects of thickness and length of specimen on liquid uptake (in Japanese). Wood Preserv 18:31–37

    Article  Google Scholar 

  13. Iida I, Ikeuchi A, Imamura Y (1995) Liquid penetration of precompressed wood III. Effects of moisture contents of specimens and ambient temperatures while compression on liquid uptakes of softwoods and hardwoods (in Japanese). Mokuzai Gakkaishi 41:811–819

    CAS  Google Scholar 

  14. Iida I, Mori S, Nakamura Y, Sakai H, Imamura Y (1996) Liquid penetration of precompressed wood V. Effects of cyclic loading, type of impregnated chemicals and annual ring angles on the uptake of water or oily solvents (in Japanese). Mokuzai Gakkaishi 42:581–588

    CAS  Google Scholar 

  15. Watanabe U, Imamura Y, Iida I (1998) Liquid penetration of precompressed wood VI: anatomical characterization of pit fractures. J Wood Sci 44:158–162

    Article  Google Scholar 

  16. Iida I, Yusuf S, Watanabe U, Imamura Y (2002) Liquid penetration of precompressed wood VII: combined treatment of precompression and extraction in hot water on the liquid penetration of wood. J Wood Sci 48:81–85

    Article  CAS  Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Satoshi Fukuta.

Additional information

Part of this report was presented at the 16th Annual Meeting of the Chubu Branch of the Japan Wood Research Society in Matsumoto, November 2006

Rights and permissions

Reprints and permissions

About this article

Cite this article

Fukuta, S., Asada, F. & Sasaki, Y. Manufacture of compressed wood fixed by phenolic resin impregnation through drilled holes. J Wood Sci 54, 100–106 (2008). https://doi.org/10.1007/s10086-007-0920-x

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s10086-007-0920-x

Key words