Table 5 Correlation coefficients between wood mass loss and n-hexane-extractive, putative juvabione, or unknown compound contents in seven todomatsu half-sib families

From: Diversities of decay resistance and n-hexane-extractive contents in seven half-sib families from plus trees in todomatsu (Abies sachalinensis)

 

ML in Fomitopsis palustris

ML in Trametes versicolor

Air-dry density

−0.104 (0.824)

−0.088 (0.851)

n-Hexane-extractive content

0.189 (0.685)

−0.535 (0.216)

Putative juvabione content

0.173 (0.711)

−0.640 (0.122)

Unknown compound content

0.083 (0.860)

−0.092 (0.844)

  1. Values in parentheses indicate probability. Correlation coefficients were determined using mean values of the percentage of wood mass loss and the contents in each half-sib family
  2. ML mass loss