Table 3 Lignin-derived dimeric products in water-soluble portion and their retention times and MS fragments for GC–MS analysis

From: Characterization of lignin-derived products from Japanese cedar as treated by semi-flow hot-compressed water

No.

Retention time (min)

Product

MS fragments (m/z)

20

38.7

Stilbene type (β-1)

272, 240, 226, 212, 198, 180, 170, 152, 138, 77, 66

21

41.4

 

281, 274, 260, 230, 214

22

42.3

 

278, 275, 245, 160, 153, 124, 109, 78, 66, 52

23

43.2

 

290, 152, 139, 124, 108, 94, 78, 66

24

43.7

 

429, 377, 356, 301, 273, 160, 153, 124, 96, 78, 66, 53

25

43.9

 

311, 300, 287, 272, 256, 240, 161, 152, 95, 78, 67

26

44.3

Phenylcoumaran type (β-5)

272, 241, 225, 213, 212, 199, 169

27

45.0

 

303, 273, 153, 124, 108, 82, 78, 66, 53

28

45.7

 

358, 313, 298, 282, 253, 210, 181, 162, 79, 52

29

46.9

 

357, 341, 313, 286, 269, 208, 175, 160, 152, 137, 78

30

47.7

 

344, 326, 312, 207, 139, 121, 93, 78, 66

31

48.8

Biphenyl type (5-5′)

326, 312, 298, 266, 190, 177, 162, 139, 124, 104, 92, 78

32

49.0

 

314, 298, 252, 239, 178, 138, 95, 78

33

51.1

 

327, 324, 312, 135, 130, 78