Table 5 Analysis of variance results of surface roughness values

From: Surface roughness and brightness of scots pine (Pinus sylvestris) applied with water-based varnish after densification and heat treatment

Factors

Degrees of freedom

Sum of squares

Mean square

F value

Level of significance (P ≤ 0.05)

Densification (A)

4

2.448

0.612

12.2296

0.0000*

Heat treatment (B)

2

21.359

10.680

213.4007

0.0000*

Interaction (AB)

8

0.514

0.064

1.2838

Ns

Varnish type (C)

2

391.861

195.930

3915.0548

0.0000*

Interaction (AC)

8

4.072

0.509

10.1703

0.0000*

Interaction (BC)

4

1.097

0.274

5.4786

0.0003*

Interaction (ABC)

16

0.728

0.046

0.9093

Ns

Error

315

15.764

0.050

  

Total

359

437.843

   