Official Journal of the Japan Wood Research Society
\( \bar{x} \) (µm) | HG | LSD | |
---|---|---|---|
Densification | |||
Undensified | 1.919 | A* | ±0.07333 |
A1 | 1.822 | B | |
A2 | 1.784 | B | |
B1 | 1.767 | B | |
B2 | 1.665 | C | |
Heat treatment (°C) | |||
190 | 1.546 | C | ±0.05680 |
200 | 1.704 | B | |
210 | 2.124 | A* | |
Varnish type | |||
Unvarnished | 3.265 | A* | ±0.05680 |
OCW | 0.997 | C | |
TCW | 1.112 | B |