Fig. 3From: Detection of decay damage in iron-wood living trees by nondestructive techniquesStress wave velocity tomogram and the corresponding stress wave velocity map grids (3 × 3 cm) of a damaged tree (no. 8, velocity range, 731–2102 m/s)Back to article page