Table 3 Comparisons of k cp and Z values for CF mats and WS mats

From: Density dependence in the thermal conductivity of cellulose fiber mats and wood shavings mats: investigation of the apparent thermal conductivity of coarse pores

 

k cp [W/(mK)]

Z

CF mats

 28–44 kg/m3

0.026 (0.025)

0.47

 44–60 kg/m3

0.026 (0.025)

0.46

WS mats

 60–80 kg/m3

0.046 (0.044)

0.22

 80–100 kg/m3

0.039 (0.039)

0.31

WSBIP

 80–120 kg/m3

0.045 (0.045)

0.61

  1. Values in parenthesis were obtained from regression curves
  2. WSBIP wood shaving binderless insulation panel [14]