Official Journal of the Japan Wood Research Society
Concentration of impregnated solution | Oven-dried samples before treatment | Samples just before conditioning | Samples after all processes | |
---|---|---|---|---|
U (mass%) | Mass m O (g) | Volume v O (cm3) | Swelling coefficient for RTb cross section α(0) (%) | Mass m V (g) |
10 | 0.859 ± 0.002a | 2.972 ± 0.021 | 6.979 ± 0.149 | 1.070 ± 0.005 |
20 | 0.857 ± 0.001 | 2.985 ± 0.003 | 6.850 ± 0.071 | 1.319 ± 0.001 |
30 | 0.856 ± 0.012 | 2.952 ± 0.033 | 6.900 ± 0.033 | 1.577 ± 0.023 |
40 | 0.862 ± 0.006 | 2.989 ± 0.019 | 6.953 ± 0.062 | 1.886 ± 0.015 |
50 | 0.858 ± 0.008 | 2.968 ± 0.022 | 7.191 ± 0.111 | 2.187 ± 0.012 |