Skip to main content

Official Journal of the Japan Wood Research Society

Table 1 Concentrations of sodium, potassium, magnesium, and calcium ions eluted from Japanese oak charcoal (OC) and water-extracted Japanese oak charcoal (nWE-OC) after 1, 4, 8, and 12 treatments

From: Cesium adsorption from aqueous solutions onto Japanese oak charcoal III: effects of water-extraction treatment

Adsorbent

Molar concentration (mol/L)

Na+

K+

Mg2+

Ca2+

OC

7.0 × 10−6

1.6 × 10−3

7.7 × 10−5

7.8 × 10−5

1WE-OC

1.3 × 10−6

8.4 × 10−4

5.3 × 10−5

1.8 × 10−4

4WE-OC

<1.3 × 10−6

5.9 × 10−4

1.7 × 10−5

3.6 × 10−4

8WE-OC

<1.3 × 10−6

3.9 × 10−4

5.8 × 10−6

1.7 × 10−4

12WE-OC

<1.3 × 10−6

3.5 × 10−4

4.5 × 10−6

1.0 × 10−4