Table 2 Power law model parameters for Chinese fir wood in all orthotropic directions

From: Application of time–temperature superposition principle to Chinese fir orthotropic creep

Specimens

J 0 (GPa−1)

k

a × 10−3 (s−1)

RMS error (%)

L

0.09

0.51

11.17

0.00

R

3.33

0.28

1.99

0.00

T

6.85

0.30

2.12

0.01

  1. J 0, initial compliance; k and a, power law parameters; RMS error, root mean square error between modeled and measured compliance values