Skip to main content

Official Journal of the Japan Wood Research Society

Table 3 Results of the pullout resistance of 30 mm welded depth for different pretreated methods

From: Influence of welded depth and CuCl2 pretreated dowels on wood dowel welding

Group

Maximum value (N)

Minimum value (N)

Mean value (N)

Standard deviation

Variable coefficient (%)

Group A-30

2290

1536

1857

228

12.28

Group B

6094

3006

4697

872

18.57

Group C

1400

404

924

275

29.76

  1. Group A-30 meant the untreated group, and the number 30 meant the welded depth 30 mm
  2. Group B meant the treated group with wood dowels immersed in CuCl2 for 30 min
  3. Group C meant the treated group with wood dowels immersed in CuCl2 for 7 days