Fig. 3From: Changes of major chemical components in larch wood through combined treatment of drying and heat treatment using superheated steamChanges of temperature and pressure of SHS in the reactor and temperature in the lumber during combined treatment (target conditions of steam: 0.5 MPa and 250 °C)Back to article page