Skip to main content

Official Journal of the Japan Wood Research Society

Table 3 Specimens for tensile strength of finger-jointed lamina

From: Stochastic model for predicting the bending strength of glued-laminated timber based on the knot area ratio and localized MOE in lamina

Dimensions (mm)

Gradea

Number of specimens

38 × 89 × 1800

E8 (8–9 GPa of MOE)

30

120

E10 (10–11 GPa of MOE)

30

E12 (12–13 GPa of MOE)

30

38 × 140 × 1800

E8 (8–9 GPa of MOE)

30

120

E10 (10–11 GPa of MOE)

30

E12 (12–13 GPa of MOE)

30

  1. MOE modulus of elasticity
  2. aE-rated grades are the same as for Table 1