From: Experimental study on the fire performance of straight-line dovetail joints
Number | Original section size | Reduced section size | Fire exposure time (min) | Charring rate (mm/min) | |||
---|---|---|---|---|---|---|---|
Width (mm) | Height (mm) | Width (mm) | Height (mm) | Horizontal | Vertical | ||
z10 | 160 | 241 | 150 | 230 | 10 | 0.50 | 0.55 |
z20 | 161 | 238 | 134 | 210 | 20 | 0.67 | 0.70 |
z30 | 160 | 241 | 123 | 199 | 30 | 0.62 | 0.70 |
zp30 | 160 | 241 | 130 | 215 | 30 | 0.50 | 0.43 |