Skip to main content

Official Journal of the Japan Wood Research Society

Table 1 Results of the hierarchical clustering analysis of near-infrared (NIR) spectra acquired from various heat-treated larch wood specimens

From: Classification of the hot air heat treatment degree of larch wood using a multivariate analysis of near-infrared spectroscopy

Time (h)

Temperature

160 °C

170 °C

180 °C

190 °C

200 °C

210 °C

220 °C

1

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

2

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

3

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

4

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

5

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

6

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

7

C(3)

C(3)

C(3)

C(3)

C(3)

C(3)

A(3)

8

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

A(3)

9

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

A(3)

10

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

A(3)

11

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

A(3)

12

C(3)

C(3)

C(3)

C(3)

C(3)

B(3)

A(3)