Table 4 Lignin contents and components in single-knockout mutants

From: The gene expression analysis of Arabidopsis thaliana ABC transporters by real-time PCR for screening monolignol-transporter candidates

 

Lignin (%)

 

S/G

H/G

WT

16.1 ± 0.5

(100)

0.80 ± 0.08

0.18 ± 0.03

abcg29

16.3 ± 0.5

(101)

0.71 ± 0.03

0.19 ± 0.01

abcg30

16.4 ± 0.5

(102)

0.76 ± 0.04

0.19 ± 0.05

abcg33

16.5 ± 0.6

(102)

0.67 ± 0.06

0.19 ± 0.03

abcg34

15.5 ± 0.7

(96)

0.64 ± 0.11

0.22 ± 0.07

abcg37

19.1 ± 1.4

(114)

0.80 ± 0.04

0.18 ± 0.04

  1. Lignin contents are presented as the proportion (%) of the cell wall dry weight. Data in parentheses are presented relative to the wild-type values, which were set at 100%. The pyrolyzed products used for calculating the S/G and H/G ratios are listed in Online Resource 5. Lignin contents and components were analyzed using four and three independent biological replicates, respectively