Table 4 Length of sound and decayed regions of decay-treated specimens

From: Lateral strength of nailed timber connections with decay

Specimens

Side member

Main member

t11 (mm)

t12 (mm)

t21 (mm)

t22 (mm)

S3M7-1

–

20 [S]

38 [S]

–

S3M7-2

–

20 [S]

25 [S]

13 [D]

S3M7-3

–

20 [S]

24 [S]

14 [D]

S3M7-4

–

20 [S]

19 [S]

19 [D]

S3M7-5

–

20 [S]

15[S]

23[D]

S3M7-6

–

20 [S]

12 [S]

26 [D]

S3M7-7

–

20 [S]

11 [S]

27 [D]

S3M7-8

–

20 [D]

27 [S]

11 [D]

S3M7-9

–

20 [S]

38 [D]

–

S3M7-10

–

20 [D]

38 [D]

–

S6M4-1

–

33 [S]

25 [S]

–

S6M4-2

–

33 [S]

25 [S]

–

S6M4-3

–

33 [S]

25 [S]

–

S6M4-4

–

33 [S]

25 [S]

–

S6M4-5

–

33 [S]

14 [S]

11 [D]

S6M4-6

–

33 [S]

11 [D]

14 [S]

S6M4-7

–

33 [S]

12 [S]

13 [D]

S6M4-8

27 [S]

6 [D]

25 [D]

–

S6M4-9

23 [D]

10 [S]

12 [S]

13 [D]

S6M4-10

–

33 [D]

13 [S]

12 [D]

S8M2-1

–

45 [S]

13 [S]

–

S8M2-2

–

45 [S]

8 [S]

5 [D]

S8M2-3

–

45 [S]

13 [D]

–

S8M2-4

–

45 [S]

13 [D]

–

S8M2-5

–

45 [S]

13 [D]

–

S8M2-6

–

45 [S]

13 [D]

–

S8M2-7

23 [D]

22 [S]

13 [S]

–

S8M2-8

34 [S]

11 [D]

13 [D]

–

S8M2-9

–

45 [D]

13 [D]

–

S8M2-10

–

45 [D]

13 [D]

–

  1. t11, t12, t21, and t22, see Fig. 1
  2. S sound status, D decayed status