Fig. 7From: Moisture-dependent orthotropic viscoelastic properties of Chinese fir wood in low temperature environmentRelationship between logarithm of frequency (lnƒ) at loss maximum and reciprocal of absolute temperature (1/T) for the L, R, and T specimens with different moisture content (MC)Back to article page