From: Stress relaxation behavior of wood in the plastic region under indoor conditions
Designation of specimens | Init (MPa) | 1 min (MPa) | 1 min/init |
---|---|---|---|
20-P0.5 | 3.83 | 3.47 | 0.91 |
20-P1 | 3.86 | 3.40 | 0.88 |
20-P2 | 5.00 | 4.45 | 0.89 |
30-P1.5 | 5.14 | 4.56 | 0.89 |
45-P1.5 | 5.17 | 4.42 | 0.85 |
30-PE | 2.20 | 2.11 | 0.96 |
30-P1.6A | 6.14 | 4.87 | 0.79 |
30-P1.6B | 7.53 | 6.09 | 0.81 |
90-P1.6 | 8.02 | 6.93 | 0.86 |
30-FE | 0.88 | 0.80 | 0.91 |
Lag45-P2.3 | 6.41 | 5.66 | 0.88 |