Fig. 1From: Microcrack propagation in transverse surface from heartwood to sapwood during dryingSample preparation: Four specimens were derived from an end-matched stick specimen. No. 2 was used for observation, No. 1 for measuring the MC, and Nos. 3 and 4 were used for measuring the MC at two appropriate instances during dryingBack to article page