Fig. 3From: Microcrack propagation in transverse surface from heartwood to sapwood during dryingThe MC of the representative specimen. The specimens included heartwood, intermediate wood, and sapwood, for the MC measurement and CLSM observation. The MCs at 49Â min and 75Â min were measured from the divided specimensBack to article page