Table 2 Surface stiffness and modulus measured using the AFM force curve mode in the samples coated with urushi

From: Resistance of wood coated with oriental lacquer (urushi) against damage caused by subterranean termite

 

Force (nN)

Modulus (nN/nm)a

KU

13.3 ± 2.5

1.22 ± 0.13

SU

14.3 ± 2.9

1.31 ± 0.07

KSU

12.5 ± 1.6

1.25 ± 0.10

BU

13.3 ± 2.1

1.26 ± 0.18