Material | Density (g/cm3) | Compressive strength (N/mm2) | Bulk density (g/cm3) | Gypsum/water ratio (w/w) |
---|---|---|---|---|
Office paper | 1.30 ± 0.02a | 5.84 ± 0.25a | 0.100 | 2.12 |
Newspaper | 1.26 ± 0.02b | 4.78 ± 0.24b | 0.094 | 2.12 |
Magazine paper | 1.28 ± 0.02b | 4.48 ± 0.25b | 0.116 | 1.96 |
Corrugated board paper | 1.30 ± 0.01a | 5.93 ± 0.37a | 0.095 | 2.12 |
Corrugated paperboard | 1.30 ± 0.01a | 6.35 ± 0.32a | 0.098 | 2.12 |
Tetra Pak I | 1.29 ± 0.03a | 6.46 ± 0.43a | 0.108 | 2.12 |
Tetra Pak II | 1.34 ± 0.01c | 6.18 ± 0.64a | 0.115 | 2.12 |