Skip to main content

Official Journal of the Japan Wood Research Society

Table 4 Condition of enzymatic saccharification of Japanese cedar and oak

From: Delignification of softwood by glycerol from biodiesel by-product I: model reaction using glycerol and fatty acid sodium soap mixture for pretreatment on bioethanol production

Code

Symbols in Fig. 6

Substrate

Treatment conditions

Lignin content [wt%]

 

Glycerol composition

Temp. [°C]

Time [h]

Run 1

Cellulose powder

0

Run 2

Japanese cedar

37.5

Run 3

Japanese cedar

20 wt% C12 Na

250

1

11.5

Run 4

Japanese cedar

20 wt% C18:0 Na

250

1

15.5

Run 5

Japanese cedar

20 wt% C18:1 Na

250

1

9.3

Run 6

Japanese cedar

20 wt% C2 Na

250

1

31.7

Run 7

Japanese cedar

Only glycerol

250

1

35.2

Run 8

Oak

26.4

Run 9

Oak

20 wt% C18:1 Na

250

1

3.6

Run 10

Oak

20 wt% C2 Na

250

1

8.6