Official Journal of the Japan Wood Research Society
From: Determination of high-temperature and low-humidity treatment time for larch boxed-heart timber
Treatment | Surface check | Internal check | ||||
---|---|---|---|---|---|---|
Area (mm2) | Standard deviation | Sum total | Area (mm2) | Standard deviation | Sum total | |
Control | 26.30 | 24.46 | 17 | 10.00 | 2.32 | 6 |
8 h | 0.08 | 0.07 | 5 | 3.00 | 0.76 | 2 |
12 h | 0.06 | 0.04 | 3 | 0.00 | 0.00 | |
16 h | 0.02 | 0.00 | 1 | 0.00 | 0.00 |