Sample | T0 (°C) | Tmax (°C) | T50% (°C) | Char residue (%) |
Lignin | 183.2 | 374.6 | 552.9 | 42.9 |
PU | 284.4 | 316.5 | 386.1 | 21.3 |
PU/L5 | 282.1 | 320.3 | 371.5 | 22.3 |
PU/L10 | 278.2 | 323.5 | 381.4 | 22.7 |
PU/L15 | 274.7 | 325.6 | 384.1 | 23.0 |
PU/L20 | 271.7 | 328.4 | 385.9 | 24.6 |
W–PU | 257.9 | 309.0 | 362.7 | 22.7 |
W–PU/L5 | 250.8 | 312.9 | 365.5 | 23.2 |
W–PU/L10 | 249.6 | 311.5 | 371.9 | 24.7 |
W–PU/L15 | 248.7 | 311.8 | 373.2 | 26.6 |
W–PU/L20 | 248.2 | 311.0 | 396.7 | 31.3 |