Table 6 Total amount of primary VOCs released per m3 of wood during conventional and high-temperature drying for plantation Pinus sylvestris and Russian Pinus sylvestris

From: Study of VOCs release during drying of plantation-grown Pinus sylvestris and naturally grown Russian Pinus sylvestris

VOCs

Amount of VOCs (mg/m3 of wood)

Plantation Pinus sylvestris

Russian Pinus sylvestris

Conventional

High temperature

Conventional

High temperature

n-Propanal

25.59

68

3.48

5.26

n-Hexanal

26.86

267.1

4.49

46.64

n-Valeraldehyde

27.65

47.3

2.59

42.57

Benzaldehyde

1.09

20.42

3.24

17.28

α-Pinene

100.24

623.83

90.5

115

β-Pinene

2.48

106.68

5

31.49

Camphene

3.46

30.04

3.97

Myrcene

1.2

87.01

2.68

4.14

Limonene

6.41

36.63

3.32

59.63

1-Heptene

4.05

6.71

1.22

12.47

Benzene

84.99

Propylbenzene

0.49

5.46