Fig. 3From: Development of colorless wood via two-step delignification involving alcoholysis and bleaching with maintaining natural hierarchical structureLignin content monitored by IR spectroscopy with increasing temperature during alcoholysis. The plots correspond to Samples 11–18 in Table 1. The error bars indicate the standard deviation calculated from 3 samplesBack to article page