Table 4 Microfibril angle, crystalline index and full-width at half-maximum of untreated and colorless wood

From: Development of colorless wood via two-step delignification involving alcoholysis and bleaching with maintaining natural hierarchical structure

 

Microfibril angle (Âş)

Crystallinity index

Full-width at half-maximum of (200) (Âş)

Untreated wood

3.22

0.56

3.18

Colorless wood

3.54

0.63

2.50