Fig. 4 | Journal of Wood Science

Fig. 4

From: Thermal reactivity of hemicellulose and cellulose in cedar and beech wood cell walls

Fig. 4

Recovery rates of hydrolysable sugars from: a Japanese cedar and b Japanese beech woods after heating to various temperatures (10 °C/min, no holding period), under a nitrogen flow (100 mL/min). Black circle glucose (Glu), black pointing-up triangle xylose (Xyl), black square mannose (Man), white circle arabinose (Ara), white pointing-up triangle galactose (Gal), white square 4-O-methyl-d-glucuronic acid (4-O-MeGlcA)