From: Thermal reactivity of hemicellulose and cellulose in cedar and beech wood cell walls

Fig. 5

Influence of pyrolysis temperature on recovery rates for: a xylose, b 4-O-MeGlcA, c mannose, d arabinose and e galactose in Japanese beech (black circle) and Japanese cedar (white circle) woods, compared with isolated xylan (white pointing-up triangle: Na+ salt, black pointing-up triangle: free carboxyl) and isolated glucomannan (x). Pyrolysis conditions: heating rate (10 °C/min)/nitrogen flow (100 mL/min)/no holding period