Fig. 7From: Effects of residual lignin and cellulose swelling on the rate of enzymatic saccharification of softwood and hardwood acid sulfite pulpsEnzymatic saccharification of delignified pulp with the enzyme dose at 3.2 FPU/g: a larch SP and b acacia SP. Open diamond: filter paper, black circle and gray circle: larch SP with a kappa number 64.3 and 127, respectively, black square and gray square: acacia SP with a kappa number 23.0 and 57.9, respectively, open circle and open square: delignified SP prepared from larch SP with the kappa number 64.3 and acacia SP with the kappa number 23.0, respectively. Enzymatic treatment: pulp 50 mg, acetate buffer pH 4.5 and 1.5 mL and temperature at 45 °CBack to article page