Skip to main content

Official Journal of the Japan Wood Research Society

Table 2 Drying rate of MW-pretreated and control samples in different drying stages

From: Effects of microwave pretreatment on drying of 50 mm-thickness Chinese fir lumber

Sample

Drying rate (%/hr)

Early stage (MC > FSP)

Later stage (MC < FSP)

Whole process

Pretreated quarter-sawn

0.337

0.129

0.188

Control quarter-sawn

0.232

0.116

0.173

Pretreated flat-sawn

0.393

0.135

0.210

Control flat-sawn

0.280

0.117

0.180