Table 3 MC and residual stress index of MW-pretreated and control samples after drying

From: Effects of microwave pretreatment on drying of 50 mm-thickness Chinese fir lumber

Sample

Final MC (%)

Drying uniformity (%)

MC deviation in the thickness (%)

Residual stress index (%)

Pretreated quarter-sawn

Control quarter-sawn

8.55

9.23

 ± 0.54

 ± 0.87

1.34 ± 0.46

2.58 ± 1.17

1.29 ± 0.44

2.26 ± 0.85

Sig.

 

*

*

Pretreated flat-sawn

Control flat-sawn

8.02

9.01

 ± 0.43

 ± 0.62

1.03 ± 0.27

1.51 ± 0.38

1.28 ± 0.82

2.49 ± 0.88

Sig.

*

 

*

*

  1. Values of drying uniformity are standard deviations of the final MC. * Means significant at 0.05 level, — Means not significant at 0.05 level