Table 1 The microfibril angle (MFA) and relative content of cellulose and lignin for compression wood (CW) and opposite wood (OW). Values in parenthesis are the coefficients of variation (%)

From: Comparative studies on wood structure and microtensile properties between compression and opposite wood fibers of Chinese fir plantation

Samples

MFA (°)

Cellulose (%)

Lignin (%)

CW

25.1 (7.79)

42.64 (1.18)

36.43 (0.83)

OW

11.5 (2.43)

46.89 (0.43)

32.81 (0.75)