Fig. 9From: Thermal degradation of hemicellulose and cellulose in ball-milled cedar and beech woodRecovery rates of hydrolyzable sugars, cellulose-derived glucose ( ), mannose ( ) and xylose ( ), following pyrolysis of ball-milled cedar and beech wood for 10 min and 4 hBack to article page