Table 2 The weight percentage of the SiC in the R–SiC samples

From: The one-step pyrolysis process of rattan-based silicon carbide multiphase ceramics prepared by sol–gel method

Sample

Temperature

(℃)

time

(min)

SiC

Cross section (%)

Longitudinal section (%)

1

1300

120

3.82 ± 0.02

1.11 ± 0.01

2

1400

120

8.58 ± 0.11

3.47 ± 0.04

3

1500

120

44.24 ± 0.44

18.29 ± 0.18

4

1500

60

39.28 ± 0.29

12.81 ± 0.01

5

1500

30

8.35 ± 0.15

6.87 ± 0.12