Table 3 Average and standard deviation of characteristic values obtained by the test

From: Embedment properties of Japanese cedar (Cryptomeria japonica) treated with resin impregnation

Group

Stiffness (kN/mm)

Proportional limit load (kN)

Yield load (kN)

N0

9.76 ± 4.93

4.60 ± 0.53

6.43 ± 0.87

U0

36.88 ± 7.87

7.63 ± 0.86

No data

A0

22.16 ± 4.39

5.09 ± 1.03

(7.01 ± 1.60)

N90

7.38 ± 2.06

2.03 ± 0.45

3.28 ± 0.52

U90

14.33 ± 3.32

4.98 ± 0.89

7.70 ± 0.87

A90

9.18 ± 2.28

3.09 ± 0.87

5.25 ± 1.20

  1. Yield load of group A0 can be obtain from 18 specimens out of 20 specimens