Table 1 The relationship between lignin removal and treatment time

From: The effect of delignification ratio on the PMMA occupation in poplar wood cell wall by the macro and micro comparative study

Time (h)

Lignin content (wt %)

Lignin removal (%)

0

22.8 (0.9)

0

6

18.83 (1.27)

17.4

9

15.98 (2.2)

29.9

12

11.01 (1.76)

51.7

18

6.11 (0.22)

73.2

24

0.62 (0.03)

97.3

  1. Values in parentheses are standard deviations