Official Journal of the Japan Wood Research Society
From: The effect of delignification ratio on the PMMA occupation in poplar wood cell wall by the macro and micro comparative study
Simples
SBET (m2/g)
Vtotal (× 10–3 cm3/g)
PMMA/DW-0
0.9975
3.482
PMMA/DW-17.4
1.1676
3.560
PMMA/DW-29.9
1.4671
2.623
PMMA/DW-51.7
0.5046
1.848
PMMA/DW-73.2
0.5848
2.288
PMMA/DW-97.3
0.2946
1.526