Fig. 4From: High pressure facilitates delignification of Japanese cedar in supercritical methanolComposition of the methanol-insoluble residue after supercritical methanol treatment [room temperature to 270 °C (8 °C/min) and at 270 °C for 30 min] of holocellulose of Japanese cedar at various pressures (values in parentheses are percentages of the composition of untreated holocellulose)Back to article page