Skip to main content

Official Journal of the Japan Wood Research Society

Table 2 Peak temperature of DTG curves of the urushi (UR) film

From: Improving the lightfastness and thermal stability of black urushi (oriental lacquer) by kraft lignin oleate

Sample

Peak temperature of DTG curves/°C

UR

317

455

UR-KL-1

316

452

UR-KL-5

316

454

UR-KL-10

294

453

KL powder

187

387

UR-OL-1

320

459

UR-OL-5

316

451

UR-OL-10

314

451

OL powder

244

365