From: Thermal softening properties of various wood species within an annual ring
Features of anatomy | Species | Density (g/cm3) |
---|---|---|
Softwood | ||
Gradual transition | Abies sachalinensis (Fr. Schmidt) masters | 0.42 |
Pinus radiata D.Don | 0.47 | |
Abrupt transition | Pseudotsuga menziesii (Mirb.) Franco | 0.50 |
Pinus densiflora Siebold et Zucc. | 0.60 | |
Cedrus deodara (Roxb.) G.Don | 0.63 | |
Hardwood | ||
Ring-porous wood | Albizia julibrissin Durazz. | 0.47 |
Castanea crenata Siebold et Zucc. | 0.54 | |
Diffuse-porous wood | Zanthoxylum ailanthoides Siebold et Zucc | 0.44 |
Populus alba L. | 0.47 |