Fig. 3From: Bending responses of self-shaping wood bilayers: comparison between adsorption and desorption processesThe bending evolution of bilayers manufactured from the monolayers with 12% iMC when the relative humidity increased from dry (0% RH) to a wet environment (95% RH) at 25 °C. Tp, the thickness of passive layer; m, passive to active layer thickness ratioBack to article page