Fig. 6From: Moisture content estimation of green softwood logs of three species based on measurements of flexural vibrationComparison of regression lines for correlation between E/ρ and tan δ for air-dried hinoki (10% moisture content) and moisture-conditioned hinoki (27%) from previous studies [16] and hinoki green heartwood (30%) in this studyBack to article page