Skip to main content

Official Journal of the Japan Wood Research Society

Table 5 Fundamental properties of oil palm wood

From: Developing structural sandwich panels for energy-efficient wall applications using laminated oil palm wood and rubberwood-based plywood/oriented strand board

Properties

Density of oil palm wood

LD

MD

Swelling (%)

  

 Tangential direction

3.8 ± 0.9 (n = 10)

7.6 ± 3.5 (n = 10)

 Radial direction

3.9 ± 1.3 (n = 10)

8.4 ± 3.6 (n = 10)

 Longitudinal direction

1.4 ± 0.5 (n = 10)

1.4 ± 0.6 (n = 10)

Shear strength parallel to grain (MPa)

1.6 ± 0.6 (n = 30)

2.0 ± 0.9 (n = 30)

Compressive strength parallel to grain (MPa)

4.8 ± 2.7 (n = 30)

12.1 ± 3.6 (n = 30)