Official Journal of the Japan Wood Research Society
Products/specie | Density | Compression | Tension | Shear | Flexural | f b/ρ | |||
---|---|---|---|---|---|---|---|---|---|
ρ | f c∥ | f c⊥ | f t∥ | f t⊥ | f s∥ | f b | E b | ||
kg/m3 | MPa | MPa | MPa | MPa | MPa | MPa | MPa | 104 m2 s−2 | |
Scrimber | 885 | 101 | 21 | 108 | 3.4 | 17 | 140 | 22,310 | 15.8 |
Sitka spruce [28] | 383 | 36 | – | 59 | – | 9 | 67 | 8000 | 17.5 |
SPF glulam [29] | 408 | 28 | 4 | – | 1.2 | 3.5 | 32 | 12,175 | 7.8 |
Douglas-fir LVL [30] | 520 | 57 | – | 49 | – | 11 | 68 | 13,000 | 13.1 |
Glubam [31] | 800–980 | 51 | – | 82 | – | – | 99 | 10,400 | 10.1–12.4 |
Glulam Guadua [32] | 741 | 62 | – | 143 | 3.2 | 9.5 | 122.4 | 13,260 | 16.5 |