Fig. 4From: Self-healing coatings for inhibiting corrosion of ferrous metals exposed to preservative-treated bambooOptical micrographs of the healed region on self-healing coatings after a 0 and b 4 days; SEM micrographs of the healed region on self-healing coating; c self-healing coatings; d control coatingsBack to article page