Table 7 Failure modes of the N-finity Moso bamboo

From: Mechanical properties of laminated bamboo lumber N-finity according to ISO 23478-2022

Testing group

Testing direction

Specimen no.

Failure modes

1

2

3

Group a

Parallel-to-grain (axial)

16

16

16

0

Group b

Perpendicular-to-grain (tangential)

16

0

0

16

Group c

Perpendicular-to-grain (radial)

16

0

0

16