Sources | Origin | Nb of samples | Max Cambial Age (years) | Sampling height (m) | Nb of cells per ring | Lumen diameter (μm) | Fibre width (μm) | Cell wall thickness (μm) | Fibre length (mm) |
---|---|---|---|---|---|---|---|---|---|
[43] | Bordeaux, France | / | 24–35 | 1.3 | 40–70 | 5–50 | / | 3–9 | / |
[44] | Tocha, Portugal | 10 | / | / | 20–60 | 5–45 | / | 3–9 | / |
[39] | / | 2 | 16–30 | / | / | / | 25–35 | 1–6 | / |
[45] | Tocha, Portugal | 33 | / | 1.3 | 24–30 | / | / | 3.5–7 | / |
[46] | Tuscany, Italie | / | / | 1.3 | / | / | / | 2–8 | / |
[47] | Tronquats, France | 960 | 14 | / | / | / | 42.5 | / | 1988 |
[38] | Aquitaine, France | 186 | 15 | / | / | / | 27.43 | / | 1990 |